Bicomponent High Efficiency Warm-keeping Cotton is made by mixing polypropylene superfine fiber and three-dimensional hollow terylene short fiber.Terylene is hollow and curling,the fiber has well flexibility and obturator structure,adhering with polypropylene fibre through heat fusion,thus makes the fibre net has well three-dimensional solid net structure,has better consolidation, integrality and fluffiness of "work-keeping, comfort,light,anti-mould",makes the worm-keeping garment be in top grade and fashion. Bicomponent worm-keeping cotton has high resilience,anti-moisture,not shoes,cap,and also other industries,such as auto industry.
Technical Dates
Type | Basic W. | Thickness | War- keeping | Heat-transfer coefficient | Clo value |
G/㎡ | mm | (rate) | (W/㎡℃) | ㎡℃/W | |
BN-40 | 40 | 0.91 | 54.68 | 11.28 | 0.577 |
BN-60 | 60 | 1.35 | 57.2 | 8.136 | 0.795 |
BN-80 | 80 | 1.99 | 65.54 | 5.197 | 1.2 |
BN-100 | 100 | 2.12 | 75.28 | 3.201 | 2.16 |
BN-150 | 150 | 3.26 | 84.37 | 2.29 | 2.808 |
BN-200 | 200 | 3.46 | 87.35 | 1.79 | 3.598 |
Performance
1.The material is whiteness soft,the solid net structure consolidated by mixing two kinds of fibres, it has comparable larger area and lighter weight;
2.Comparing with normal fibre,bicomponent fibre has higher block function for emanation of heat quantity,has better worm-keeping effect;
3.The material is easily dry after dampening,its moisture regain rate is close to zero,is suitable to be used under damp and cold environment;
4.It is mixed by two kind fibres with different diameter,has well flexibility,can be used for worm-keeping and sound insulation in the auto industry.
Ingredient of the Bicomponent Fibers High Efficiency Warm-keeping Cotton
Terylene 25%,polypropylene 75%